The Stabilization of Waste Funnel Glass of CRT by SiO 2 Film Coating Technique

Author

Listed:
  • Jyh-Herng Chen

    (Department of Materials and Mineral Resources Engineering, National Taipei University of Technology, 1, Section 3, Chung-Hsiao E. Rd., Taipei 10608, Taiwan)

  • Yu-Hao Chang

    (Department of Materials and Mineral Resources Engineering, National Taipei University of Technology, 1, Section 3, Chung-Hsiao E. Rd., Taipei 10608, Taiwan)

  • Chaochin Su

    (Department of Molecular Science and Engineering, National Taipei University of Technology, Daan, Taipei 10608, Taiwan)

  • Kai-Chung Hsu

    (Department of Materials and Mineral Resources Engineering, National Taipei University of Technology, 1, Section 3, Chung-Hsiao E. Rd., Taipei 10608, Taiwan)

Abstract

The funnel glass of the CRT monitor contains about 22–28% of lead oxide, of which lead is a highly toxic species and hazardous to the environment. This study proposes a process to form a protective layer of SiO 2 film coating on the funnel glass to reduce the hazardous effect of lead leaching to the environment. The film coating benefits from the advantages of the sol–gel method. There are two key procedures of the stabilization technique, including the alkaline treatment and the formation of SiO 2 coating from TEOS. The results show that the funnel glass powder treated with 10 M NaOH can produce a mushy layer on the surface. The mushy layer, which comprises OH − and water, can promote the formation of the SiO 2 film layer on the surface of funnel glass powder. The conditions of the SiO 2 film coating proposed in this study are: alkaline treatment by 10 M NaOH, the addition ratio of TEOS and funnel glass powder 2: 1, reaction temperature 40 °C, and reaction time 1.3 h. The EDS and ESCA results show that the Pb peak intensity on the surface of funnel glass decreases with the film coating. In the TCLP test, the leaching amount for Pb of the SiO 2 film coated funnel glass powders is 0.7 mg/L, which is far lower than the standard in Taiwan EPA. Based on the experimental results, the formation mechanism of the SiO 2 film layer on the surface of waste funnel glass powder is proposed. This study demonstrates that the SiO 2 film coating is a potentially effective method to solve the problem of the waste funnel glass.

Suggested Citation

  • Jyh-Herng Chen & Yu-Hao Chang & Chaochin Su & Kai-Chung Hsu, 2021. "The Stabilization of Waste Funnel Glass of CRT by SiO 2 Film Coating Technique," Sustainability, MDPI, vol. 13(16), pages 1-12, August.
  • Handle: RePEc:gam:jsusta:v:13:y:2021:i:16:p:9096-:d:614082
    as

    Download full text from publisher

    File URL: https://www.mdpi.com/2071-1050/13/16/9096/pdf
    Download Restriction: no

    File URL: https://www.mdpi.com/2071-1050/13/16/9096/
    Download Restriction: no
    ---><---

    References listed on IDEAS

    as
    1. Alvaro Blanco & Emmanuel Chomski & Serguei Grabtchak & Marta Ibisate & Sajeev John & Stephen W. Leonard & Cefe Lopez & Francisco Meseguer & Hernan Miguez & Jessica P. Mondia & Geoffrey A. Ozin & Ovidi, 2000. "Large-scale synthesis of a silicon photonic crystal with a complete three-dimensional bandgap near 1.5 micrometres," Nature, Nature, vol. 405(6785), pages 437-440, May.
    2. Edmond Chow & S.Y. Lin & S.G. Johnson & P.R. Villeneuve & J.D. Joannopoulos & J.R. Wendt & G.A. Vawter & W. Zubrzycki & H. Hou & A. Alleman, 2000. "Three-dimensional control of light in a two-dimensional photonic crystal slab," Nature, Nature, vol. 407(6807), pages 983-986, October.
    Full references (including those not matched with items on IDEAS)

    Most related items

    These are the items that most often cite the same works as this one and are cited by the same works as this one.

      Corrections

      All material on this site has been provided by the respective publishers and authors. You can help correct errors and omissions. When requesting a correction, please mention this item's handle: RePEc:gam:jsusta:v:13:y:2021:i:16:p:9096-:d:614082. See general information about how to correct material in RePEc.

      If you have authored this item and are not yet registered with RePEc, we encourage you to do it here. This allows to link your profile to this item. It also allows you to accept potential citations to this item that we are uncertain about.

      If CitEc recognized a bibliographic reference but did not link an item in RePEc to it, you can help with this form .

      If you know of missing items citing this one, you can help us creating those links by adding the relevant references in the same way as above, for each refering item. If you are a registered author of this item, you may also want to check the "citations" tab in your RePEc Author Service profile, as there may be some citations waiting for confirmation.

      For technical questions regarding this item, or to correct its authors, title, abstract, bibliographic or download information, contact: MDPI Indexing Manager (email available below). General contact details of provider: https://www.mdpi.com .

      Please note that corrections may take a couple of weeks to filter through the various RePEc services.

      IDEAS is a RePEc service. RePEc uses bibliographic data supplied by the respective publishers.