Author
Listed:
- Jinlin Wang
(Peking University)
- Yun-Qin Li
(East China Normal University)
- Rui Wang
(Peking University)
- Qi Liu
(Peking University)
- Haotian Ye
(Peking University)
- Ping Wang
(Peking University)
- Xifan Xu
(Peking University)
- Huaiyuan Yang
(Peking University)
- Fang Liu
(Peking University)
- Bowen Sheng
(Peking University)
- Liuyun Yang
(Peking University)
- Xiaoyang Yin
(Peking University)
- Yi Tong
(Suzhou Laboratory)
- Tao Wang
(Peking University
Peking University)
- Wen-Yi Tong
(East China Normal University)
- Xin-Zheng Li
(Peking University
Peking University
Peking University
Peking University Yangtze Delta Institute of Optoelectronics)
- Chun-Gang Duan
(East China Normal University
East China Normal University)
- Bo Shen
(Peking University
Peking University
Peking University Yangtze Delta Institute of Optoelectronics)
- Xinqiang Wang
(Peking University
Peking University
Peking University Yangtze Delta Institute of Optoelectronics)
Abstract
Wurtzite ferroelectrics hold immense promise to revolutionize modern micro- and nano-electronics due to their compatibility with semiconductor technologies. However, the presence of interfacial dead layers with irreversible polarization limits their development and applications, and the formation mechanisms of dead layers remain unclear. Here, we demonstrate that dead layer formation in ScAlN, a representative wurtzite ferroelectric, originates from a high density of nitrogen vacancies in combination with interfacial strain. Atomic-scale investigations using scanning transmission electron microscopy (STEM) and electron energy loss spectroscopy (EELS), supported by first-principles calculations, reveal that compressive strain near the ScAlN/GaN interface reduces the formation energy of nitrogen vacancies, promoting their generation. These vacancies degrade dielectric properties and raise the ferroelectric switching barrier, the latter further exacerbated by compressive strain. These combined effects suppress polarization reversibility near the interface. This work elucidates the microscopic origin of interfacial dead layers and highlights the significance of defect and strain engineering in wurtzite ferroelectrics, which are essential to advancing their integration and scalability in next-generation electronic devices.
Suggested Citation
Jinlin Wang & Yun-Qin Li & Rui Wang & Qi Liu & Haotian Ye & Ping Wang & Xifan Xu & Huaiyuan Yang & Fang Liu & Bowen Sheng & Liuyun Yang & Xiaoyang Yin & Yi Tong & Tao Wang & Wen-Yi Tong & Xin-Zheng Li, 2025.
"Unveiling interfacial dead layer in wurtzite ferroelectrics,"
Nature Communications, Nature, vol. 16(1), pages 1-10, December.
Handle:
RePEc:nat:natcom:v:16:y:2025:i:1:d:10.1038_s41467-025-61291-2
DOI: 10.1038/s41467-025-61291-2
Download full text from publisher
Corrections
All material on this site has been provided by the respective publishers and authors. You can help correct errors and omissions. When requesting a correction, please mention this item's handle: RePEc:nat:natcom:v:16:y:2025:i:1:d:10.1038_s41467-025-61291-2. See general information about how to correct material in RePEc.
If you have authored this item and are not yet registered with RePEc, we encourage you to do it here. This allows to link your profile to this item. It also allows you to accept potential citations to this item that we are uncertain about.
We have no bibliographic references for this item. You can help adding them by using this form .
If you know of missing items citing this one, you can help us creating those links by adding the relevant references in the same way as above, for each refering item. If you are a registered author of this item, you may also want to check the "citations" tab in your RePEc Author Service profile, as there may be some citations waiting for confirmation.
For technical questions regarding this item, or to correct its authors, title, abstract, bibliographic or download information, contact: Sonal Shukla or Springer Nature Abstracting and Indexing (email available below). General contact details of provider: http://www.nature.com .
Please note that corrections may take a couple of weeks to filter through
the various RePEc services.